Executive Gov
  • Home
  • Acquisition & Procurement
  • Agencies
    • Department of War
    • Intelligence Community
    • DHS
    • Federal Civilian
    • Space
  • Cybersecurity
  • Technology
  • News
  • About
  • Wash100
  • Contact Us
    • Advertising
    • Submit your news
No Result
View All Result
Executive Gov
  • Home
  • Acquisition & Procurement
  • Agencies
    • Department of War
    • Intelligence Community
    • DHS
    • Federal Civilian
    • Space
  • Cybersecurity
  • Technology
  • News
  • About
  • Wash100
  • Contact Us
    • Advertising
    • Submit your news
No Result
View All Result
Executive Gov
No Result
View All Result
Home News

4 Companies Secure Licenses to Produce NASA’s 3D-Printable Superalloy

by Naomi Cooper
May 11, 2024
in News, Space
GRX-810 superalloy_272x270

GRX-810 superalloy_272x270

NASA has agreed to license an advanced superalloy developed for complex air and spaceflight environments to four companies in a move to make the invention available to aviation and space industry parts manufacturers.

Table of Contents

  • You might also like
  • Army Forms PM ATSR to Unify Aerial, Ground Sensor Acquisitions
  • DOJ Stands Up Super Intelligence Task Force to Counter AI Misuse
  • DOW Commits $150M Conditional Loan to LeoLabs to Scale Space Radar Production

You might also like

Army Forms PM ATSR to Unify Aerial, Ground Sensor Acquisitions

DOJ Stands Up Super Intelligence Task Force to Counter AI Misuse

DOW Commits $150M Conditional Loan to LeoLabs to Scale Space Radar Production

The agency said Thursday it has entered into co-exclusive license agreements with Carpenter Technology, Elementum 3D, Linde Advanced Material Technologies and Powder Alloy Corporation to produce and market GRX-810, a 3D-printable high-temperature material developed under NASA’s Transformational Tools and Technologies project.

“NASA invests tax dollars into research that demonstrates direct benefit to the U.S. and transfers its technologies to industry by licensing its patents,” said Amy Hiltabidel, licensing manager at NASA’s Glenn Research Center.

The superalloy is capable of enduring temperatures higher than 2,000 degrees Fahrenheit, making it a strong candidate for building aerospace components and parts like liquid rocket engine injectors, combustors and turbines.

“GRX-810 represents a new alloy design space and manufacturing technique that was impossible a few years ago,” said Tim Smith, materials researcher at NASA Glenn.

Smith and his Glenn colleague Christopher Kantzos invented the superalloy by employing a time-saving computer modeling and laser 3D printing process that fuses metals together, layer by layer.

Stay connected via Google News
Follow us for the latest travel updates and guides.
Add as preferred source on Google
Share5Tweet19
Previous Post

Foundation for Energy Security and Innovation Board Members Announced

Next Post

Lawrence Livermore to Provide Space Imaging Payload for Space Force’s Victus Haze Mission

Recommended For You

Army Works to Implement Autonomous Swarms in Operations

by Nichols Martin
September 5, 2019
Army Works to Implement Autonomous Swarms in Operations

Army Futures Command has been studying the use of unmanned systems to form tactical swarms that would support small units of soldiers. The service branch said Wednesday it...

Read moreDetails

Construction Begins on New National Advanced Air Mobility Center of Excellence in Ohio

by Naomi Cooper
September 2, 2022
Construction Begins on New National Advanced Air Mobility Center of Excellence in Ohio

The construction of the new National Advanced Air Mobility Center of Excellence at Springfield-Beckley Municipal Airport in Ohio has begun with a groundbreaking ceremony held on Aug. 23.The...

Read moreDetails

White House Unveils Contracting, Security Assistance Transparency Commitments Under 3rd Open Govt Action Plan

by Jane Edwards
September 25, 2024
White House Unveils Contracting, Security Assistance Transparency Commitments Under 3rd Open Govt Action Plan

The White House has announced seven new initiatives as part of the Third Open Government National Action Plan that seeks to promote transparency, innovation and accountability in the...

Read moreDetails

Senators Propose Bill to Permanently End Government Shutdowns

by Darwin McDaniel
January 15, 2019
Senators Propose Bill to Permanently End Government Shutdowns

Republican lawmakers have introduced a bill to the Senate to permanently end the implementation of a government shutdown. The End Government Shutdowns Act would create an automatic continuing resolution...

Read moreDetails

Commerce Dept to Reorganize AI Safety Institute to Advance AI Development

by Kristen Smith
June 5, 2025
Commerce Dept to Reorganize AI Safety Institute to Advance AI Development

The Department of Commerce has announced plans to rebrand the AI Safety Institute into the Center for AI Standards and Innovation to address hindrances to advancing the development...

Read moreDetails
Sign Up For Our Newsletter
Subscribe to our mailing list to receives daily updates direct to your inbox!
Invalid email address
Your privacy is guranteed.
Thanks for subscribing!

Sponsors

About ExecutiveGov

ExecutiveGov, published by Executive Mosaic, is a site dedicated to the news and headlines in the federal government. ExecutiveGov serves as a news source for the hot topics and issues facing federal government departments and agencies such as Gov 2.0, cybersecurity policy, health IT, green IT and national security. We also aim to spotlight various federal government employees and interview key government executives whose impact resonates beyond their agency.

CATEGORIES

  • Acquisition & Procurement
  • Announcements
  • Articles
  • Artificial Intelligence
  • Australia
  • Awards
  • Big Data & Analytics News
  • C4ISR
  • C5ISR
  • Cloud
  • Contract Awards
  • Cybersecurity
  • Defense And Intelligence
  • Defense Security Cooperation
  • Department of War
  • DHS
  • Digital Assets
  • Digital Modernization
  • Emerging Tech
  • Events
  • Executive Moves
  • Executive Spotlights
  • Federal Civilian
  • Financial Reports
  • Foreign Military Sales
  • General News
  • GovCon Expert
  • Government Cloud
  • GSA
  • Healthcare IT
  • Industry News
  • Intelligence Community
  • Legislation
  • M&A Activity
  • Middle East
  • National Security
  • News
  • Policy Updates
  • Press Releases
  • Profiles
  • Space
  • Technology
  • Videos
  • Wash100
Sign Up For Our Newsletter
Subscribe to our mailing list to receives daily updates direct to your inbox!
Invalid email address
Your privacy is guranteed.
Thanks for subscribing!

Copyright 2026 Executive Mosaic. All Rights Reserved. Site Archive

No Result
View All Result
  • Home
  • Acquisition & Procurement
  • Agencies
    • Department of War
    • Intelligence Community
    • DHS
    • Federal Civilian
    • Space
  • Cybersecurity
  • Technology
  • News
  • About
  • Wash100
  • Contact Us
    • Advertising
    • Submit your news

Copyright 2026 Executive Mosaic. All Rights Reserved. Site Archive

Get your free GovCon news!

Get your latest GovCon news and insights. Become a VIP and subscribe to the GovConWire Daily News.

Invalid email address
We promise not to spam you. You can unsubscribe at any time.
Thanks for subscribing!